Pinhole Leaks in Copper Pipes Figure 6

Figure 6.   Pitting corrosion in 3/4 inch horizontal cold water tube left stagnant for several months following testing and flushing.

Figure 6.   Pitting corrosion in 3/4 inch horizontal cold water tube left stagnant for
several months following testing and flushing.